データセット名:2023_Biobased polymers for 3D printing Orthodontic appliances_FE-SEM

課題名:Biobased polymers for 3D printing Orthodontic appliances

データセット登録者(所属機関):ZUNIGA, Enrique Ezra(Health Sciences University of Hokkaido)

課題番号:
JPMXP1223CT0126
実施機関:
公立千歳科学技術大学

要約

The increase in the use of 3D printers in orthodontic treatment, and the expectation of a further increase in the future, has raised concerns about the environmental impact due to the disposal of 3D printing resin materials, which are mostly derived from petroleum resources. In response, this study aims to develop 3D printable polymer materials from environmentally friendly biomass and biodegradable raw materials, and to investigate the possibility of using sustainable materials in 3D printing in dentistry.
Epoxidised soya oil acrylate and epoxidised soya oil methacrylate were synthesized and used as the base materials, alongside tetrahydrofurfuryl methacrylate (THFMA) and isobornyl methacrylate (IBOMA) serving as diluents. Phenylbis-2,4,6-trimethylbenzoylphosphine oxide (BAPO) was utilized as a photoinitiator to synthesize four different light-curing resins. Test specimens were prepared from these synthesized resins and were compared against four dental 3D printing materials. The specimens underwent FE-SEM observations.

CM3

キーワード・タグ

重要技術領域(主):
重要技術領域(副):
横断技術領域:
マテリアルインデックス:
キーワードタグ:

データメトリックス

ページビュー:
33
ダウンロード数:
0

データインデックス

https://doi.org/10.71947/arim.jpmxp1223ct0126-1
登録日:
2026.04.21
エンバーゴ解除日:
2026.03.31
データセットID:
12e0cbfc-664f-4027-b123-2fb404bf7215
データタイル数:
11
ファイル数:
116
ファイルサイズ:
47.43MB
ライセンス:
ARIMライセンス

成果発表・成果利用