データセット名:希土類フリー/低希土類永久磁石材料の開発(多目的X線回折装置)_FY2023

課題名:希土類フリー/低希土類永久磁石材料の開発

データセット登録者(所属機関):SEPEHRI AMIN, Hossein(NIMS)

課題番号:
JPMXP1223NM5332
実施機関:
物質・材料研究機構

要約

Magnetic materials are essential component for the green energy conversions. The functionality of magnetic materials is realized by engineering the magnetic and thermal hysteresis. In this research, we have investigated materials with lean from rare-earth with excellent intrinsic magnetic properties and conducted microstructure and alloy design to convert excellent intrinsic magnetic properties to the extrinsic ones, in particular hysteresis control of the materials. This research is focused on permanent magnets as well as magnetocaloric materials for efficient magnetic cooling.
We have used XRD (SmartLab (45 kV, 200 mA, CuKα, Rigaku)) and study the phase transition behavior of the materials at a wide temperature range.

23NM5332_NM-204.png

キーワード・タグ

重要技術領域(主):
重要技術領域(副):
横断技術領域:
マテリアルインデックス:
キーワードタグ:

データメトリックス

ページビュー:
42
ダウンロード数:
0

データインデックス

https://doi.org/10.71947/arim.jpmxp1223nm5332
登録日:
2026.04.23
エンバーゴ解除日:
2026.03.31
データセットID:
c4147dc1-12b8-4c4b-b770-c5a11998530c
データタイル数:
4
ファイル数:
536
ファイルサイズ:
219.46MB
ライセンス:
ARIMライセンス

成果発表・成果利用