利用報告書 / User's Reports

  • 印刷する

【公開日:2023.07.28】【最終更新日:2023.05.25】

課題データ / Project Data

課題番号 / Project Issue Number

22TU0027

利用課題名 / Title

Crystallization behavior of metallic glasses

利用した実施機関 / Support Institute

東北大学 / Tohoku Univ.

機関外・機関内の利用 / External or Internal Use

外部利用/External Use

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)高度なデバイス機能の発現を可能とするマテリアル/Materials allowing high-level device functions to be performed(副 / Sub)-

キーワード / Keywords

バルクアモルファス合金,電子顕微鏡/Electron microscopy


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

Louzguine Dmitri Valentinovich

所属名 / Affiliation

産業技術総合研究所 オープンイノベーションラボラトリ

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

TU-516:分析電子顕微鏡
TU-517:透過電子顕微鏡


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

Structural features of the Pd42.5Cu30Ni7.5P20 and Pt42.5Cu27Ni9.5P21 metallic glasses are studied in the present work by high-resolution transmission electron microscopy. The results indicate that Pd42.5Cu30Ni7.5P20 is a true bulk glass-former containing no crystalline particles/nuclei, while Pt42.5Cu27Ni9.5P21 is a crystal growth-controlled type bulk glass-former which contains nanoparticles of about 1 nm size with a different chemical composition. These structural differences are manifested in room-temperature mechanical properties. Thermodynamic calculations are also used to support the observed features.

実験 / Experimental

Ingots of the Pd42.5Cu30Ni7.5P20 and Pt42.5Cu27Ni9.5P21 alloys (the compositions are given in nominal atomic/molar percentages) were prepared by smelting of pure elements of 99.9 % mass purity. The structures of the samples were examined by conventional X-ray diffractometry (XRD) with CuKa radiation. Transmission electron microscopy observation, including collection of selected-area electron diffraction (SAED) and nanobeam diffraction (NBD) (1 nm probe size) patterns were carried out using a TOPCON EM-002B microscope operating at 160 kV. Scanning TEM (STEM) observation and the energy-dispersive X-ray (EDX) analysis were performed using JEOL-ARM200F microscope operating at 200 kV.  Oxygen content in the studied glassy alloys was measured by using infrared absorption (IA) after fusion under He gas.

結果と考察 / Results and Discussion

Significant difference in fine structure of the Pd42.5Cu30Ni7.5P20 and Pt42.5Cu27Ni9.5P21 metallic glasses was found (Figs. 1 and 2). The Pd42.5Cu30Ni7.5P20 metallic glass is a true bulk glass-former containing no crystalline particles/nuclei (Fig. 1), while the Pt42.5Cu27Ni9.5P21 metallic glass contains cF4 (partially ordered as cP4) nanoparticles (Fig. 2) both in bulk and ribbon form. This peculiar structure is rather the origin of much higher plasticity of Pt-based BMGs compared to Pd-based ones in general, and in the present case. Moreover, the microstructure analysis with a complex mathematical approach provided accurate data and enlightened the structure features of a known metallic glass. The analysis of EDX maps indicated that these nanoparticles are enriched in Cu and Ni and depleted in Pt and P. Low spatial correlation with O indicated that these nanoparticles are not oxides. Thermodynamic calculations support the observed features.

図・表・数式 / Figures, Tables and Equations


Fig.1 High-resolution TEM (HRTEM) (a) and STEM bright-field (b) images of the Pd42.5Cu30Ni7.5P20 metallic glass in ribbon form, together with a nanobeam diffraction pattern (inset).



Fig.2 High-resolution TEM (HRTEM) (a) and STEM bright-field (b) images of the Pt42.5Cu27Ni9.5P21 metallic glass in ribbon form, together with a nanobeam diffraction pattern (inset).


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

印刷する
PAGE TOP
スマートフォン用ページで見る