利用報告書 / User's Reports

  • 印刷する

【公開日:2023.07.28】【最終更新日:2023.04.27】

課題データ / Project Data

課題番号 / Project Issue Number

22NM0043

利用課題名 / Title

グラフェンに関する研究

利用した実施機関 / Support Institute

物質・材料研究機構 / NIMS

機関外・機関内の利用 / External or Internal Use

外部利用/External Use

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)物質・材料合成プロセス/Molecule & Material Synthesis(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)革新的なエネルギー変換を可能とするマテリアル/Materials enabling innovative energy conversion(副 / Sub)次世代ナノスケールマテリアル/Next-generation nanoscale materials

キーワード / Keywords

エネルギー貯蔵/ Energy storage,ナノチューブ/ Nanotube,ナノ多孔体/ Nanoporuous material,電極材料/ Electrode material


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

張 坤

所属名 / Affiliation

株式会社マテリアルイノベーションつくば

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)技術代行/Technology Substitution(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

NM-504:200kV電界放出形透過電子顕微鏡(JEM-2100F2)


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

To put a few layers of graphene and graphene oxide films on carbon/metal materials with high coverage, the hydrophilization treatment of carbon/metal materials is a key.

実験 / Experimental

In this study, the effect of plasma treatment on the hydrophilization of surfaces of carbon/metal materials is examined. The plasma hydrophilization function of an Au coater was used in this study. TEM samples were prepared by dropping ca. 20 μL of the graphene oxide dispersion onto a holey carbon mesh grid and drying under 120 °C in a vacuum oven. TEM images were observed by a JEOL 2100 TEM with an operating voltage of 200 kV.

結果と考察 / Results and Discussion

By dropping pure water containing graphene oxide flakes on carbon/metal substrates immediately after 25 sec hydrophilization treatment, a few layers graphene oxides could cover on the carbon/metal substrates with high coverage. When quantifoil is used as a grid, the hydrophilic treatment for 180 s can make 1-7 layers of graphene oxide uniformly cover the grid as shown in Fig.1. And the coverage can reach 80%.

図・表・数式 / Figures, Tables and Equations


Fig.1 TEM images of samples.


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

印刷する
PAGE TOP
スマートフォン用ページで見る