利用報告書 / User's Reports

  • 印刷する

【公開日:2023.07.31】【最終更新日:2023.05.16】

課題データ / Project Data

課題番号 / Project Issue Number

22UT0431

利用課題名 / Title

ポリマーフィルムの表面分析

利用した実施機関 / Support Institute

東京大学 / Tokyo Univ.

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)マルチマテリアル化技術・次世代高分子マテリアル/Multi-material technologies / Next-generation high-molecular materials(副 / Sub)-

キーワード / Keywords

Organic functional materials,電子顕微鏡/Electron microscopy


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

Jeong SungYeob

所属名 / Affiliation

東京大学

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

UT-102:高分解能走査型分析電子顕微鏡


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

Characterization of conductive graphitized material fabricated on the surface of polymer films through laser irradiation

実験 / Experimental

A transparent polymer surface is irradiated with femtosecond laser pulses at a specific scanning speed, resulting in the fabrication of linear conductive electrodes.

結果と考察 / Results and Discussion

It has been confirmed that a laser fluence of ~20 J/cm^2 with a scanning speed of 20 mm/sec is the most suitable preprocessing condition for subsequent studies. Additionally, at scanning speeds below 10 mm/sec, graphitized materials were not formed on the surface; instead, partial ablation occurred, creating a channeled and pitted surface that was unsuitable for experimentation.

図・表・数式 / Figures, Tables and Equations


Laser-induced graphene fabrication with laser fluence of 20 J/cm^2 and scanning speed of 3 mm/sec.



Laser-induced graphene fabrication with laser fluence of 20 J/cm^2 and scanning speed of 20 mm/sec.



Laser-induced graphene fabrication with laser fluence of 20 J/cm^2 and scanning speed of 100 mm/sec.


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)

The paper has not yet been published.


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

印刷する
PAGE TOP
スマートフォン用ページで見る