Developement of functional amphiphilic block copolymers through self assembly of hydrogen-bonding moieties

利用した実施機関 / Support Institute

東京大学 / Tokyo Univ.

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)マルチマテリアル化技術・次世代高分子マテリアル/Multi-material technologies / Next-generation high-molecular materials(副 / Sub)-

キーワード / Keywords

Organic functional materials, polymer materials,電子顕微鏡/ Electronic microscope


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

Lang Rongjian

所属名 / Affiliation

東京大学 大学院工学系研究科

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes

Takashi Kato

ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes

Ryosuke Teranishi

利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

UT-011:有機材料ハイコントラスト透過型電子顕微鏡


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

In this research project, we aimed to control the nanostructure and create new functions using the self-organization of block copolymers. We mainly investigated the morphology and size of these nanoaggregates formed in water using scanning and transmission electron microscopy.

実験 / Experimental

Transmission electron microscopy (TEM) observations were conducted to examine the morphology and size of the aggregates in water. Each polymer dispersion was stained with phosphotungstic acid solution and dropped onto a carbon-supported copper grid that had been hydrophilized using a JEOL HDT-400. Observations were performed using a JEOL JEM-1400 at an acceleration voltage of 120 kV.

結果と考察 / Results and Discussion

By introducing intermolecular interactions other than hydrophobic interactions into diblock amphiphilic block copolymers and by varying the molecular weight of block copolymers, it was suggested that the morphology, size, and size distribution of self-organized nanostructures on the sub-micron to sub-nano scale could be controlled.

図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)