利用報告書 / User's Reports

  • 印刷する

【公開日:2024.07.25】【最終更新日:2024.06.29】

課題データ / Project Data

課題番号 / Project Issue Number

23UT0283

利用課題名 / Title

ヒト血清アルブミンに対する高親和性を持つ分子インプリントポリマーナノ粒子の基本的特性

利用した実施機関 / Support Institute

東京大学 / Tokyo Univ.

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)次世代ナノスケールマテリアル/Next-generation nanoscale materials(副 / Sub)-

キーワード / Keywords

電子分光/ Electron spectroscopy,ナノ粒子/ Nanoparticles


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

満 又源

所属名 / Affiliation

東京大学 大学院工学系研究科マテリアル専攻

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

UT-308:多機能走査型X線光電子分光分析装置(XPS)with AES


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

Molecularly imprinted polymer nanopaticles (nano-MIPs) imprinting human serum albumin (HSA) were developed and applied to ISFET biosensor with a Ta2O5 gate insulator. Specifically, nano-MIPs were used as analytes and interacted with HSA-coated ISFET biosensor. Therefore, the chemically modified interface of this biosensor needed assessment using XPS. A dopamine layering chemistry recently developed in our lab was assessed as well. 

実験 / Experimental

To ensure measurement precision, the samples were characterized over 10 cycles  included 5 scans of N 1s, a single scan each of C 1s and Ta 4f, and 10 scans of S 2p. The measurements were conducted with a pass energy of 27 eV, and peak positions were calibrated against adventitious carbon (284.5 eV) for accuracy. 

結果と考察 / Results and Discussion

The Ta4f region exhibits well-separated spin-orbit components with an energy separation of 1.9 eV. This separation, along with the peak positions at ~26.2 eV for 4f 7/2 and 4f 5/2, is indicative of Ta2O5 [1]. The energy separation and peak area ratios support this, with the latter of 1.33 also revealing the electron configuration of Ta 4f, characterized by a spin-orbit split (Fig 1.). As the surface chemistry progressed, a notable decrease in peak intensity was observed, especially after the immobilization of Human Serum Albumin (HSA). This trend suggests the successful alteration of the surface chemistry. Like in the Ta 4f region, the Ta 4p 3/2 peak overlapping with N 1s region followed the same trend throughout the surface chemistry phases [2]. The initiation of the chemistry with dopamine layering introduced new peaks adjacent to the Ta 4p 3/2 peak, attributable to the introduction of nitrogen (Fig 2.). Although subtle peaks of chemical states of nitrogen might be masked by the Ta 4p 3/2 peak, the nitrogen peaks were still further analyzed using Gaussian fitting, revealing dual Gaussian peaks for each phase after the initiation of the chemistry. For the dopamine layering and subsequent crosslinking with glutaraldehyde, two distinct peaks were identified, correlating to -NH2 and -NH chemical states [3]. After dopamine layering process, the peak area ratio of -NH2 to -NH was 2.26, illustrating a composition of 70% -NH2 and 30% -NH. This distribution changes after crosslinking to a ratio of 0.42, indicating a transformation of 40% of NH2 groups into NH. During HSA immobilization, these peaks correspond to -NH and C-N, aligning with the chemical states of peptide chains. In the S 2p spectra, a single peak at ~164.1 eV was observed, originating from the sulfur atoms in the disulfide groups (−S−S−) between cysteine residues in HSA molecules (Fig 3.) [4]. 

図・表・数式 / Figures, Tables and Equations


Fig 1. XPS spectra of Ta 4f



Fig 2. XPS spectra of N 1s



Fig 3. XPS spectra of S 2p


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)

[1]         McLellan, R. A., et al., Adv. Sci., 2023, 2300921[2]         Liu, W.-S., et al., Appl. Surf. Sci., 459, 477-482 (2018)[3]         Ravi, S., et al., J. Ind. Eng. Chem., 67, 210-218 (2018) [4]        Zhang, Y., et al., Sci. Rep., 8, 3185 (2018)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)