利用報告書 / User's Reports

  • 印刷する

【公開日:2024.07.25】【最終更新日:2024.07.16】

課題データ / Project Data

課題番号 / Project Issue Number

23UT1226

利用課題名 / Title

高分子液滴の乾燥パターンの解明

利用した実施機関 / Support Institute

東京大学 / Tokyo Univ.

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)次世代バイオマテリアル/Next-generation biomaterials(副 / Sub)-

キーワード / Keywords

bio-medical applications,バイオアダプティブ材料/ Bioadaptive materials,走査プローブ顕微鏡/ Scanning probe microscope,光学顕微鏡/ Optical microscope


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

PAL ANUSUYA

所属名 / Affiliation

東京大学大学院総合文化研究科 (Graduate School of Arts and Sciences, The University of Tokyo)

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes

Mitsuhiro Yoda

ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub),技術補助/Technical Assistance


利用した主な設備 / Equipment Used in This Project

UT-850:形状・膜厚・電気特性評価装置群


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

AIM: To know the height of the polymer film. Use: A height profile image for various polymer films

実験 / Experimental

Exp: We deposit a drop of 2 mm diameter polymer on the glass substrate and let it dry overnight. Then, the dried film is used under this microscope to scene the 3d height profile. 

結果と考察 / Results and Discussion

Height profile maps for polymer films provide valuable insights into the surface topography and morphology of the films as shown in Fig. 1 and Fig.2. The changes in processing parameters, such as concentration, affect the morphology of polymer films, thereby influencing crack formation behavior. Height profile maps obtained from films This elucidates the relationship between processing parameters and crack formation. The Height profile maps are correlated with mechanical properties data that is obtained by optical microscopy as the dynamics of the crack propagation. This correlation enables us to understand how variations in surface morphology relate to the film's mechanical behavior, including its resistance to crack initiation and propagation. Overall, height profile maps play a crucial role in gaining the underlying mechanisms governing crack formation in polymer films, as these serve as a fingerprint of the healthy and non-healthy samples. This helps us to design a pattern recognized tool for various bio-medical applications.

図・表・数式 / Figures, Tables and Equations


Fig.1 This is the 3D profile of the polymer serum mimicking the diabetic conditions



Fig.2 This is the 3D profile of the polymer serum mimicking the condition for healthy person. 


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)

We want to thank Mitsuhiro Yoda for his valuable time and support. Without him, we could not have done these experiments and gained the insights that have a bigger impact on our research. 


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

印刷する
PAGE TOP
スマートフォン用ページで見る