課題番号 / Project Issue Number

23NU0068

利用課題名 / Title

電気化学的CO2還元用ヘテロ遷移金属単原子触媒

利用した実施機関 / Support Institute

名古屋大学 / Nagoya Univ.

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)革新的なエネルギー変換を可能とするマテリアル/Materials enabling innovative energy conversion(副 / Sub)-

キーワード / Keywords

Single atom catalyst, CO2 conversion, electrochemistry,電子顕微鏡/ Electronic microscope,環境発電/ Energy Harvesting


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

Sirisomboonchai Suchada

所属名 / Affiliation

名古屋大学大学院工学研究科

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes

Park Gi-Dong

ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes

山本悠太

利用形態 / Support Type

(主 / Main)技術代行/Technology Substitution(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

NU-102:高分解能電子状態計測走査透過型電子顕微鏡システム


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

In this study, we prepared transition metal single atom catalyst (SAC) supported on N-doped carbon with high selective for CO2R to CO. The prepared SACs manifest a well-defined graphene interconnected porous structure and highly distributed single metal sites.

実験 / Experimental

利用装置: 収差補正電子顕微鏡 (JEM-ARM 200F Cold) HR-TEM image: confirming structure of carbon matrix and formation of aggregated particles, in some cases we anticipated the formation of nickel nanoparticles.Aberration-corrected HAADF-STEM image: checking the degree of dispersion of atomically isolated metal atoms. STEM-EDS: along with the HAADF-STEM visualizing the distribution of each element, carbon, nitrogen, and transition metal.

結果と考察 / Results and Discussion

- From the HR-TEM image, we could verify the amorphous carbon structure, and excessive metal loading in preparing precursor induced the formation of metal nanoparticles.
From the HAADF-STEM image with EDS, the uniformly dispersed metal atom could be confirmed. EDS result shows the average distance between hetero transition metal atoms was 2.4 ~ 2.5 Å, that is homogeneously dispersed on the carbon matrix.

図・表・数式 / Figures, Tables and Equations


Figure


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

印刷する
PAGE TOP
スマートフォン用ページで見る