24NM5177
利用課題名 / Title
軟磁性材料の開発
利用した実施機関 / Support Institute
物質・材料研究機構 / NIMS
機関外・機関内の利用 / External or Internal Use
内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)
技術領域 / Technology Area
【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)計測・分析/Advanced Characterization
【重要技術領域 / Important Technology Area】(主 / Main)革新的なエネルギー変換を可能とするマテリアル/Materials enabling innovative energy conversion(副 / Sub)マテリアルの高度循環のための技術/Advanced materials recycling technologies
キーワード / Keywords
Magnetic materials,Inductively coupled plasma emission spectroscopy,Gas chromatography
利用者と利用形態 / User and Support Type
利用者名(課題申請者)/ User Name (Project Applicant)
セペリ アミン ホセイン
所属名 / Affiliation
物質・材料研究機構
共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
藤井 湧
利用形態 / Support Type
(主 / Main)技術代行/Technology Substitution(副 / Sub),機器利用/Equipment Utilization
利用した主な設備 / Equipment Used in This Project
NM-203:誘導結合プラズマ発光分析装置群
NM-206:酸素窒素水素分析装置、炭素硫黄分析装置
報告書データ / Report
概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)
Soft magnetic materials play an important role in power electronic applications. In this project we develop soft magnetic materials with large saturation magnetization and low core losses for high frequency power electronic applications.
実験 / Experimental
the alloys were prepared by induction melting followed by melt spinning process. The chemical composition of Fe-rich alloys were measured by ICP method.
結果と考察 / Results and Discussion
Fe-enriched amorphous ribbons with a composition of Fe84.8Si0.5B9.4P3.4Cu0.8C1.1 in at. % were fabricated using an industrial-scale rapid solidification process, demonstrating excellent quality and flexibility. The composition of alloys were measured by ICP. the ribbons were annealed at different temperatures to optimize their nanostructure followed by magnetic and core loss measurements at different temperatures.
図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)
成果発表・成果利用 / Publication and Patents
論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents
特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件