One step assembly of protein for large area 2D bionanosheets

利用した実施機関 / Support Institute

物質・材料研究機構 / NIMS

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)次世代バイオマテリアル/Next-generation biomaterials(副 / Sub)次世代ナノスケールマテリアル/Next-generation nanoscale materials

キーワード / Keywords

Atomic layer thin film, Nanosheet


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

川上 亘作

所属名 / Affiliation

物質・材料研究機構

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes

Song Jingwen

ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

NM-216:薄膜X線回折装置_Cu


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

2D bionanosheets have been selected for a variety of applications. In this experiment, we want to utilize the thin-film GI-XRD to investigate the stiffness, topography, and thickness of 2D bionanosheets.

実験 / Experimental

2D bionanosheets were immobilized on the surface silicon wafer for thin-film GI-XRD study.

結果と考察 / Results and Discussion

We want to use thin-film GI-XRD to investigate the structure properties of 2D bionanosheets. The GI-XRD patterns of the assembled nanosheets exhibit distinct diffraction peaks, indicating their ordered molecular arrangement. The primary diffraction peak at 1° corresponds to an interlayer spacing of 8.8 nm (Figure 1), calculated using Bragg’s law. Compared to the monomeric state, this suggests a more compact and periodic stacking of the nanosheets.

図・表・数式 / Figures, Tables and Equations


Figure 1. GI-XRD pattern


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

印刷する
PAGE TOP
スマートフォン用ページで見る